Steel Standard:EN 10025-3
Rolling Type:Structural steel plate,low alloy steel plate
Thickness:6mm-350mm
Width:1500mm-4200mm
Length:3000mm-18000mm
Heat Treatment:Normalised
Structural steel plate S460NL is in steel standard EN 10025-3.Normalized heat treatment and Low temperature impacting test under -50 centigrade shall be done for steel plate S460NL.For hot rolled steel plate tolerances of steel S460NL the basic requirements shall be in accordance with EN 10029, including thickness tolerances to class A, unless otherwise agreed at the time of the order.Steel plate S460NL shall be suitable for welding,and general requirements for arc welding of the steel S460NL shall be given in EN 1011-2.
Technical Requirements & Additional Services:
Low temperature impacting test
Rolling under standard NACE MR-0175 (HIC+SSCC)
Ultrasonic test under EN 10160,ASTM A435,A577,A578
Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
Shot blasting and Painting,Cutting and welding as per end user’s demands
Mechnical property for S460NL Structural steel:
Thickness (mm) | ||||||||
S460NL | ≤ 16 | > 16 ≤ 40 | > 40 ≤ 63 | > 63 ≤ 80 | > 80 ≤ 100 | > 100 ≤ 150 | > 150 ≤ 200 | > 200 |
Yield strength (≥Mpa) | 460 | 440 | 430 | 410 | 400 | 380 | 370 | 370 |
≤ 100 | > 100 ≤ 200 | > 200 | ||||||
Tensile strength (Mpa) | 540-720 | 530-710 | 530-710 |
Main chemical elements composition of S460NL | ||||||
C | Si | Mn | P | S | Nb | V |
0.20 | 0.60 | 1.00-1.70 | 0.025 | 0.020 | 0.05 | 0.20 |
Al(total) | Ti | Cr | Ni | Mo | Cu | N |
≥0.02 | 0.05 | 0.30 | 0.80 | 0.10 | 0.55 | 0.025 |